3D Printed Nickel Superalloy
Year:
2019Ranking:
Third PlaceArtist:
Jeff Rossin (Graduate Student)Department:
Materials and Mechanical EngineeringLab:
Pollock and Daly Research GroupsDescription
Electron Backscatter Diffraction Image of the grain structure of an 3D Printed Nickel Alloy. The grains are elongated in the build direction(vertical) as layers of metal powders are melted by the laser. The different colors correspond to different crystallographic orientations.